J.T. Hickinbottom Ltd | Aluminium and non-ferrous founders
Experience & ExpertiseA Comprehensive rangecontact.htmHomepage

A comprehensive range of heat treatment, and non-destructive testing is available, which is usually quoted separately when specified.
Metal Grades Weight Range

  • LM4, LM6, LM25 0.1 to 300kgs
  • ZA12 0.1 to 200kgs
  • HCC1, HCC2 0.1 to 200kgs
  • PB1, PB2 0.1 to 280kgs
  • AB1, AB2, AB3 0.1 to 250kgs
  • HTB1, HTB2, HTB3 0.1 to 280kgs
  • LPB1, LB2, LB4, LG2, LG4 0.1 to 280kgs

Other alloys not listed above, may be considered. We are always willing to discuss any specific requirement. We are normally able to use existing pattern equipment, however, patternmaking services are available. Wherever possible we like to be involved at the design stage, where we may be able to advise on cost saving.